Apart from general corrosion, stainless steel corrosion can take on several specialized forms.
Fortunately, there are ways to address most forms or avoid them entirely. The following are common forms of specialized corrosion.
1. Galling
This corrosion occurs when stainless steel parts are forced together. Commonly seen with nuts, bolts, and other fasteners, corrosion isn’t visible until the parts are separated or disassembled.
The process uses repeated passes to adjust the dimensions of the steel slowly. In most cases, this will involve rolling through multiple mills over time to achieve the desired thickness.
2. Galvanic
Also known as bimetallic corrosion, this corrosion occurs when stainless steel is used with other metals in a moist environment. Rain, condensation or other moisture sources can act as an electrolyte in the presence of an electrical current causing one metal to corrode at an accelerated rate.
Exact characteristics of galvanic corrosion vary based on metals used, temperatures, areas of contact and other factors. For more information on the topic, consulting the British Standards Institution’s PD 6484 is recommended.
3. Pitting
This corrosion is typically a result of exposure to chemicals in the environment or poor aeration. It is also more common in steels with unwanted inclusions or manufacturing defects. For example, Manganese (II) Sulfide often initiates pitting.
Adequate oxygen availability can help to reduce the rate of pitting corrosion or halt it entirely depending on the cause. Steels with molybdenum also have an increased ability to both resist pitting and slow its progress. Other considerations include pH, chloride concentration and temperature of the environment in which the steel is used.
4. Crevice Corrosion
This corrosion occurs when a crevice between the stainless steel and another material allows chlorides to concentrate or prevents proper oxygen levels to regenerate the steel’s oxide layer. While typically found near or within the gap between two metals, crevice corrosion can also occur between metallic and non-metallic surfaces.
Welding, ensuring proper drainage and using proper gaskets can also help to prevent crevice corrosion as these all help to decrease access to crevices or eliminate them altogether.
5. Weld Decay
Also known as intergranular corrosion, this corrosion results from heating stainless steel to a specific temperature range—often between 550C and 850C. This causes chromium to precipitate from the stainless steel and reduces the ability for the passivation layer to regenerate.
Using low carbon steels—such as 304L and 316L—when welding can help to reduce the impact of weld decay. Additives such as titanium or niobium can further stabilize the steel and reduce precipitation while welding. In all cases, using a post-weld heat treatment is recommended to minimize corrosion.